Technet,
I have a large (2 inch) BGA that I am designing a PWB for. Where can I find
information on how much movement from TCE (thermal coefficient of expansion) mis-match
can a solder joint be expected to live with.
I have calculated that the parts will see less than .25 mm of movement from solder
temperatures to room temperatures and .02 - .03 mm of movement over typical operational
temperature cycles. I expect the BGA to have .75 mm (30 mil) balls on it.
I am looking for something to tell me when I am "close enough", or give me some kind of
"MTBF feeling", so I can judge the risks in the design.
Thanks
George Franck
Raytheon, Falls Church Va
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|