Vernon,
Sulfur is used in the manufacturing of "brown" cardboard. The dust has a high level of
sulfur in it!
D. A. Douthit
Brooks Bill wrote:
> Mystery Sulfur.... reminds me of a problem we had once, turns out the sulfur
> was coming from a rubber compound that we were using... Don't know of any
> sulfur compounds in resisters though...
> got me! - Bill Brooks
>
> -----Original Message-----
> From: Vernon Richard [mailto:[log in to unmask]]
> Sent: Wednesday, June 14, 2000 4:12 PM
> To: [log in to unmask]
> Subject: [TN] Resistor termination disappearing
>
> Hello, TechNet!
>
> We're working a problem with a resistor where the value increases due to
> some chemical reaction. The reaction takes place between the termination
> silver and sulfur present on the component. This causes the resistor to
> change value due to the silver being depleted from the connection interface.
> We don't introduce any sulfur in our processes (std smt w/ aqueous wash, Dow
> 1753 coated), so we suspect that it comes from the resistor manufacturing
> process. We also seem to have a gap in the glassivation over the interface
> area.
>
> Has anyone seen this before? What was done to eliminate the problem? Help-
> our customer is getting very concerned!
>
> Thanks. Rick Vernon
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|