Hi Mike,
I used the AltaVista to find the following links for you....
..... Hole "tenting" is available through the via-cap process in which
PC401®, a thermally cured epoxy, is screened over the holes to be tented,
after liquid photo-imageable soldermask is applied. This is an advantage for
vacuum applications after assembly......
http://www.merix.com/resourcecntr/dfm/dfm_e.html
http://www.capitalelectro.com/capab.htm
http://www.altavista.com/cgi-bin/query?pg=q&sc=on&hl=on&act=2006&par=0&q=PC4
01+soldermask&kl=XX&stype=stext&search.x=19&search.y=14
Have a wonderful day
Very Best Regards
Roland
PCB Consultant - Company viability, Technical viability, Technology choice,
Yield improvement, Company Strategy, Equipment choice, Company acquisition
Roland Jaquet - Tel. +41-22-880-0405 - Fax. +41-22-880-0409 - Cell
+41-79-203-3723
http://members.xoom.com/rjaquet/index.htm
_______________________________________________________________________
----- Original Message -----
From: Mcmaster, Michael <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 14, 2000 2:05 AM
Subject: [TN] PC401 Soldermask
> Can anyone tell me the name of the current manufacturer of PC401
soldermask?
> I have some old documents that say Photocircuits but I don't think that's
> right. A contact, especially a Web page would be appreciated also.
Thanks.
> Mike McMaster
> RF Product Engineer
> Merix Corporation
> Forest Grove OR
> 503-992-4263
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for addition
al
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|