TECHNET Archives

June 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
multipart/mixed; boundary="------------73B0C81CD28462470A1F7C78"
Sender:
Subject:
From:
Dave Simmons <[log in to unmask]>
Date:
Tue, 13 Jun 2000 08:28:45 +1200
MIME-Version:
1.0
Organization:
Tait Electronics Ltd
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Dave Simmons <[log in to unmask]>
Parts/Attachments:
text/plain (467 bytes) , david.simmons.vcf (329 bytes)
Hi All,

We are checking placement of some PBGA's. I have an ERSAScope on a demo,
and when viewing the solder balls/joints of the BGA there is some
"scaling" on the surface of the ball.
I was wondering what this scaling is a function of (e.g. to rapid
cooling, not hot enough, to hot during reflow?), and is it a defect I
should be worried about. I am not seeing this "scaling" on any of the
other parts (QFP100, 0603 chips) on the board.
Can anyone offer any advice?
Thanks
David