Hi Jim,
What is your hole and lead diameter? We've had the
same problem and we discovered that the difference
between the two was almost three times the maximum
suggested in IPC-D-275.
The difference between the maximum hole to minimum
lead diameter should not be over 0.032".
Hope that answer your question.
JF
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Dieselberg, Ron
> Sent: Monday, June 12, 2000 8:57 AM
> To: [log in to unmask]
> Subject: Re: [TN] Solder Fill
>
>
> Just a quick guess since I don't know all of the details, but
> maybe the lead
> to hole ratio is not proper. Like small lead, big hole. The thru
> hole gurus
> can give you the exact ratios I am sure.
> Ron Dieselberg
>
> -----Original Message-----
> From: Jim Gilbert [mailto:[log in to unmask]]
> Sent: Friday, June 09, 2000 09:03
> To: [log in to unmask]
> Subject: [TN] Solder Fill
>
>
> Technetters,
>
> We have a customer that is touching up the assembly after wave solder.
> This touch up is to improve the aesthetics on holes which have not
> completely wicked up on the lead. We have explained to him that
> this isn't
> necessary and he is probably doing more damage than good, however this
> isn't the issue. The issue is that when he pulls the soldering iron away
> from the hole the solder appears to fall through the hole and wick on the
> component lead on the opposite side. We have done cross
> sectional analysis
> to ensure the holes aren't voided and the solder isn't being pulled in.
> Sections look good with a consistent ounce of plating in the holes. I am
> unsure of what the hole sizes are that he's having problems with, but
> obviously something is awry with the solder "falling out". Any ideas on
> what cause may be?
>
> Thanks in advance for your help.
>
> Jim Gilbert
> Electronic Circuits & Design
> Sebring, Ohio
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|