hi,
here's the reply. i'm not sure what this means other than that the boards need to be bagged in a non-silver tarnish container. i believe the threat of silver migration is mitigated by its extreme thinness. i have the feeling that these people at lucent are fabbing their own pwb's in-house.
it still looks like a good candidate for an evaluation. if there are more messages related to this, i'll pass them on.
phil
-----Original Message-----
From: Wenger, George M (George) [mailto:[log in to unmask]]
Sent: Wednesday, June 07, 2000 10:49 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion White Tin
Darrel,
We think IAg is different that the thick silver plating that is used on
components. The IAg thickness on our boards is about 6 microinches thick.
It will tarnish extensively (i.e., turn back in color) if exposed to sulfur
so we don't expose it to S and if it does get exposed we don't use the
boards.
Most people miss the reason we use IAg. We are not using it as a solderable
surface!. We are using it as a visual inspection to know that the copper
features should be solderable (i.e., if the copper features change from a
copper color to a silver color during IAg plating than the copper wasn't
contaminated with solder mask residue or tin-strip residue from the board
fabrication process.
Regards,
George
George M. Wenger DMTS
Bell Laboratories Princeton, Supply Network Solutions
Engineering Research Center FMA / AQA / RCA Lab
(609) 639-2769 (Office); 3210 (Lab); 2343 (Fax)
[log in to unmask]
-----Original Message-----
From: Darrel Therriault [mailto:[log in to unmask]]
Sent: Wednesday, June 07, 2000 10:16 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion White Tin
At 10:39 AM 6/7/00 -0400, you wrote:
>[log in to unmask]
George,
Thanks for a very insightful synopsis of IWT. I recall many years back
that silver plated ICs caused solder problems
due to tarnishing. Is IAg different from that problem?
Thanks again for the info. Very helpful.
Regards.....DT
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|