The 130'C shock (150 - 20) shock may have something to do with it .
preheated ? 30 bars won't heat up much ,
but ensures fast contact with possible CTE consequences
just a sleepy idea paul
-----Original Message-----
From: Martin Christie [mailto:[log in to unmask]]
Sent: Wednesday, 10 May 2000 21:35
To: [log in to unmask]
Subject: Re: [TN] loose components
Lon,
What do the failed solder joints look like? i.e. do they look like they have
suffered mechanical damage or have they gone through another reflow perhaps.
Is it always the same component that fails?
Martin
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
10/05/00 12:02
>Hi,
>
>Is one of you technetters familiar with this problem:
>
>For a customer we produce a board (3 by 5 centimeters)with no more then 6
>smt components 1206. When they encapsule the board with a compound one of
>the components looses from the board. They put the compound on the board
>with 30-40 bar pressure and 150deg celsius temperature. It seems to me that
>the preesure causes a higher temperature then 150 deg.
>The customer says the soldering joints are bad , but we can't find any
>solderingproblems at all.
>
>Thanks in advance
>
>Lon Weffers
>Matas Electronics bv
>De Dieze 16
>5684PT Best The Netherlands
>www.matas.nl
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|