Carl
If, by "cleaning", you mean using shop compressed air, you probably contaminate more
than clean, even if the air is desiccated and filtered. Unless you choose ultra-pure
bottled gases with carefully cleaned pipework (a whole story in itself), regulators,
etc., then you are very likely to cause more harm than good. Even then, each time you
pull the trigger, you probably cause surrounding surfaces to raise suspended dust which
will settle on everything (unless you are in a properly maintained clean room, which
should never allow an air movement to disturb the airflow, anyway). Don't know about
the ESD aspects, but my guess is those pretty orange coiled vinyl pipes look pretty
static-generating to me.
Brian
Carl Barnes wrote:
> Fellow Technetters,
>
> What is the standard(s) for ESD and air hose use(nozzles, PSI, etc.) for
> circuit board cleaning? Can't seem to find anything on the esda.org site.
>
> Any help would be appreciated. Especially any documented items that I could
> use to train our employees.
>
> Thanks,
> Carl Barnes
> Quality Analyst
> Varian Electronics Manufacturing
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|