Jesse:
The test method appears to have been written using the owner's manual
for UPA's Caviderm. CMI also makes an excellent instrument that
utilizes micro ohm resistance.
Don Vischulis
090512 ¬x¹t«H wrote:
> TechNetters;Does anybody know where can purchase the microhm
> resistance meter with standard four*probe technique that mentioned in
> IPC-TM-650 2.2.13.1 " Thickness, Plating in Holes Microhm Method"
> ?Any feedback at all would be greatly appreciated.Best Regards Jesse
> Hung
> Customer Quality Engineer
> Quality Assurance Department
> Tel:886-3-3231111 ext: 5361
> Fax:886-3-3235874
> email address: "[log in to unmask]"
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################