Magnetic permeability varies with many factors like flux density, magnetization,
polarization and temperature. Actually it's the slope dB/dH of the B-H curve of
that material. It's relatively easier to just talk about the initial
permeability (B< 10 gauss) at a particular temperature, but still I've never
heard about the existence of a mathematical function. If you want to get an idea
of how Ui varies with freqency, you may look at a magnetic core supplier's
catalog (Magnetic Inc., AVX, Philips, Siemens, Tokin, TDK, etc.). Of course it
only tells ferromagnetic material's. I can send you some scanned pages if you
want.
K.K. Chin
Artesyn Technologies,
Fremont, CA
http://www.artesyn.com
Barbara Burcham <[log in to unmask]> on 05/12/2000 09:24:05 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
Barbara Burcham <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: KK Chin)
Subject: [TN] Formula for the Permability of Materials at different
frequencies ?
Formula for the Permability of Materials at different frequencies?
Anyone out there have one of these that can be shared?
Thanks,
Barbara Burcham
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|