hi! good morning. i just want to ask what are the other possible causes of discoloration we are encountering in our line. I already check the concentration and base from analysis, it is within our standard. I also check the temperature of the bath tank (chemicals) and it is ok.
Any help would be highly appreciated. Thanks in advance.