Technetters, got a question about resistance (or surface resistivity) of static dissipative lab coats.
I've been pushing for people to keep their coats closed here, as suggested by several technetters a few weeks back.
Now one of the operators tells me, Those lab coats don't work, I tried to measure the resistance and they are no good.
So I went to our wrist and heel strap checker and found I could not get my cuff to cuff resistance to pass either wrist or heel check. It failed high. When I checked the resistance between snaps on one cuff, using a multimeter, I found 10-20 megohms. My coat is white with grey threads through it, the conductive nylon filaments, I guess. It's made from 4 or 5 or more pieces of material, like a lot of coats. There is a metal rivet in each sholder where 3 pieces of fabric come together, that looks like it's supposed to connect the nylon from the various pieces.
Can anyone comment on my experience?
Lou Hart
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|