TECHNET Archives

May 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Shirley Xiao <[log in to unmask]>
Date:
Tue, 9 May 2000 22:15:31 -0700
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Shirley Xiao <[log in to unmask]>
Parts/Attachments:
text/plain (50 lines)
 We use standard FR-4 laminate (Tg=130 C) to produce
1.6 mm thick double sided PCB for a telecom-switch-box
customer (laminate construction is 8X7628 with H/H
copper foil) . My customer require warpage less than
0.7% after reflow and wave soldering because the cards
need to be inserted into slots of machine racks. They
are looking for warpage less than 0.5% in three
months. We tried three different laminate vendors, but
in the end all have about 6% fall out of 0.7% after
reflow and wave soldering. My customer confirmed that
their reflow & wave process is under control. The
laminate vendors said use standard FR-4 laminate
(Tg=130 C) will  lead to certain percentage fall out
of 0.7% (so that IPC-4101 defines laminate warpage
less than 1.0% for 1.6mm thick laminate).
   My questions are:
   1. Is it true that use standard FR-4 laminate are
sure to have certain percentage >0.7% warpage?
   2. Is it true that use high Tg FR-4 laminate will
have better warpage result?
   3. What material is recommended by IPC-D-275 and
IPC-D-279 for SMT board? Is high Tg preferred? (Sorry
I don't have IPC-D-275 & IPC-D-279 on hand)

   Any comments will be greatly appreciated!!!

   Thanks in advance!!!

   Shirley Xiao


__________________________________________________
Do You Yahoo!?
Send instant messages & get email alerts with Yahoo! Messenger.
http://im.yahoo.com/

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2