As was stated in earlier replies, indeed the Gold bath is very aggressive.
Before we changed to our current Resist (Dupont, and no, not a plug for
them) we often had to bake the resist prior to any Gold plating. Your resist
supplier should have some data on this for the asking.
Franklin
----- Original Message -----
From: Frank Barber <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, April 25, 2000 1:19 PM
Subject: [TN] Gold leakage under Dryfilm
> I have a question,
>
> Why would I see gold leakage under my dryfilm, when none of my
other
> plating leaks? (Including my sulfmate nickle!) Any replies as to where to
> start looking would be appreciated.
>
>
> Thank You,
>
> Sal
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|