Good Morning Technet
Hope that a few of the "all knowing, all powerful" are available for
questions
and not all out at IPC. I have been tasked with a corrective action on
a
16 layer board, .125 thick that exhibited some outgassing during
leveling.
I lost 4 or 5 of a run of 30. Where should I start to look for the
culprit? All
normal bake cycles were observed (at least signed off on the work
order).
Somebody give me a clue?!?
Anne Ledger
EMDS, Inc
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################