Jason,
a friend of mine, who has calculated the life of solderings for Volvo, has set the limit of tempcycles to a number that makes my ordinary MIL/SPACE/Telecom-experience jitter hysterically! He has written a lot about the matter. Interested to speak with him?
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: Jason Larson, CET [mailto:[log in to unmask]]
Sent: den 6 april 2000 01:13
To: [log in to unmask]
Subject: [TN] Reliability Engineering - Automotive
I am looking for information on what should be done during simulated
environmental testing of product, such as what parameters to measure, should
alterations be made to the product for test purposes, is trying to measure
the resistance of a solder joint an appropriate test measure.
Any help would be great
Jason
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|