Hi technet, I need help to investigate a failed component issue.
Some history first;
* Received modules back from warranty return for analysis,
* performed electrical testing on modules and found current
measurement on one of the pins to be higher than typical,
* dissected the potting compound away from the component ( 1N4751 30 v
zener ) associated with that part of the circuit,
* the diode measurement was incorrect for this component ( i.e.
measured .23 volts in both directions ), there is a cap in parallel with the
diode but compared the reading to a known good module and the cap doesn't
affect the reading,
* then viewed the component under stereoscope and noticed the glass
package had cracked and there was discoloration with the component
- sent away a couple of the units to the diode manufacture for failure
analysis
- requested mtbf data from manufacturer on diode
- reviewed insertion process for any indication if the ai process was the
root cause,
- 100 % of finished goods rechecked to verify the current draw was typical,
found no nc's
The modules are enclosed in a plastic case and then potted with polyurethane
( Conathene En-2521 ) for weather resistance
sample size of 12 put through validation phase that included thermal shock
and vibration, this failure mode was not evident in these modules ( this was
done before the modules were mass produced )
The 30 v zener is used in conjunction with other components as a transient
suppresser,
What I am wondering is,
* is this application suitable for a zener?
* will the diode crack from electrical stress?
* is there a chemical available that will breakdown the potting
compound without harming components (currently I place the module in the
thermal chamber and heat it up then carefully pick away the compound for the
circuit area that I am interested in)
* are there any ideas on how to get this fault to replicate this
failure in-house
Thanks for any suggestions, I am new to the manufacturing arena and
unfortunately there are no mentors in failure analysis in the company to
learn from.
Jason
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|