Jean-François
Teflon is a funny stuff. Because it is sintered (fritté) and not moulded onto the
copper wire, it can be quite porous, depending on the quality of the sintering. You may
find considerable variations in dielectric strength (and constant) from one make of
wire to another or even between batches from the same manufacturer. It is not really
suitable for high voltage use, especially if you bend it with a radius smaller than
about 20 mm. It is also hell for triboelectric effects.
Brian
Jean-Francois Bissonnette wrote:
> Hello Technetters,
>
> Can anyone tell me what is the dielectric resistance
> of teflon? We use a 22 AWG teflon wire that frequently
> fails Hi-Pot (high voltage: 1400V).
>
> JF
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|