A question for the PCB gurus:
We have been receiving boards from a supplier that are exhibiting
separations at the interface between plated hole wall and internal layers
(a.k.a. interplane separations, post separations, interconnect defects) in
cross-section, after thermal stress. Specifically, the separations are
occurring between the electroless copper and electrolytic copper. Horizontal
cross-sectioning reveals that the location of the separations is consistent
from hole to hole. For example, in a grouping of holes viewed in horizontal
cross-section, the majority of holes will show the separation extending from
the 6 o'clock position to the 11 o'clock position. Any suggestions on what
process/processes the vendor should look to for troubleshooting?
Thanks,
David Smith
Benchmark Electronics
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|