I need to find some fab shops with the following capabilities:
Board thickness: 0.125" - 0.250"
Blind and buried vias
Plated closed, silver filled holes with smooth surface pads (via in pad)
Epoxy plugged vias (for vacuum protection)
Drill to trace: 0.005"
Trace width/space: 0.004/0.004"
Low quantities: 2-10 boards
Non-plated aspect ratio: 30:1
Plated aspect ratio: 25:1
Full body gold
40 layers
Dielectric thickness 0.004 to 0.020"
Controlled impedance : 50, 55, 75, 105, 150 ohms
In house high resolution TDR measurements
Leakage to 2000 MOhms
Netlist test
FR-4, Cynate ester, Getek, polyimide
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|