Gary,
To look at literature availablr, go to www.rampinc.com, then go to Library
Resources and click on Free Downloads. Search for 'Fretting' . There are
three references listed on fretting in connectors and solutions on how to
prevent it.
For lubrication of connectors, why you wait for 24 hours? The contact lube
I have used at my past employer allowed the contacts to be mated after lube
with out waiting.
What kind of lube you are using?
----- Original Message -----
From: "Gary Camac" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, April 07, 2000 7:03 AM
Subject: [TN] Contact Lubricant and Fretting Corrosion
> Good morning everyone,
>
> I had a couple of questions concerning the prevention of fretting
corrosion. I am in the
> process of reviewing and updating some of our older process procedures.
At present the
> procedure on Lubrication of Connectors is setting in front of me and I
have managed to
> raise a few questions. A search of the Technet archives and some old
memory banks have
> produced: gold to gold - its a good thing, no lubricant required: tin/lead
to tin/lead -
> its a good thing if lubricated: gold to tin/lead - not good, even with
lubrication. I
> know some of the information on this subject is dated, but I don't believe
the passing of
> time has invalidated it.
>
> On products where we build the entire assembly, I can easily verify the
total connector
> configuration. However, when we are building only a circuit board
assembly for a
> customer, I have no idea of materials used in the mating connectors. To
further
> complicate the issue, I know that some connector manufacturers lubricate
the tin or
> tin/lead female connectors and some manufacturers do not, or at least
won't verify that
> they do.
>
> Is there an industrial specification/requirement for the lubrication of
connectors on
> circuit board assemblies that should be called out in the product
specification?
>
> At present we are using a contact lubricant on all tin or tin/lead plated
male connector
> contacts, except when the mating connector is known to be prelubricated.
The lubricant we
> are using must be allowed to cure out 24 hours prior to assembly. This is
not real
> conducive to lowering cycle times. Is anyone aware of a contact lubricate
the would
> improve on this?
>
> Thanks,
>
> Gary Camac
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|