Pa5r and Mike;
I have been told here in Brazil that recycled solder dross will not be
returned to solder wave process, but goes to automotive or lamp industries.
The reason is recovered dross didn't achieve the purity level for the alloy
63/37 and then this solder is changed to other alloys ( 60/40, etc ) and is
sold to other aplications with this money a brand new processed alloy is
transfered to you.
Maybe our process here is not as good as this equipment should be.
Another question arrives here.
Do you believe that the solder vendor will accept the dross from the
Solder Recovery System ?
Thanks
Jorge Dourado de Santana
Maintenance / Process Engr
Microtec - Brazil
> -----Original Message-----
> From: McMonagle, Mike [SMTP:[log in to unmask]]
> Sent: 7 de Abril de 2000 08:38
> To: [log in to unmask]
> Subject: Re: [TN] Dross recycling
>
> John,
> Look at the Earthtronics Solder Recovery System at
> http://www.fancort.com/. Fancort is the stateside distributor of this UK
> developed system. There's also a link to Earthronics site, which contains
> a
> variety of case studies from major manufacturers. On average, you can
> expect
> a 50% reclaim of good solder from dross using this system.
>
> Mike McMonagle
> PCBA Process Engineering
> Telxon Corporation
> (713) 307-2443 Phone
> (713) 307-2581 Fax
> www.telxon.com
>
> ' Innovative Solutions for
> Mobile Information and
> Wireless Communications'
>
>
> -----Original Message-----
> From: parrrrr rossss [mailto:[log in to unmask]]
> Sent: Friday, April 07, 2000 5:05 AM
> To: [log in to unmask]
> Subject: [TN] Dross recycling
>
>
> Hi,
>
> I have a question about dorss recycling :
>
> Is there any off-line equipment in market
> to separate the good solder from the dross ( waste
> collected from the wave solder pot) ?
>
> John
>
>
>
> __________________________________________________
> Do You Yahoo!?
> Talk to your friends online with Yahoo! Messenger.
> http://im.yahoo.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|