Metals in solution are too low in electrons, and thus have a positive charge.
Solid metals, in their shiney form, have the proper number of electrons.
When a more "active" metal (meaning a metal that does not bind its electrons
tightly) is immersed into a solution of a metal that does bind its electrons
tightly, like Gold, the electrons shift from the substrate metal, (the
substrate under Gold is almost always Nickel) to the metal in solution,
causing the metal in solution to plate out spontaneously on to the substrate
metal....in other words, a Nickel coated PCB, when immersed into a solution
of Gold, will cause the Gold to plate out spontaneously on to the Nickel, and
in the process some of the Nickel is dissolved and goes into solution.
This continues until the substrate Nickel is covered, and no more Nickel is
available for this chemical reaction, and you wind up with around 7-8
microinches (0.2 micron) of Gold from this type of plating.
Hope this helped...
Rudy Sedlak
RD Chemical Company
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|