Brighteners /carriers concentration can be analyzed by qualiplate CVS (cyclic
voltametric stripping). However for gold plating baths this does not apply.
Usually brighteners in gold plating baths are not being analyzed, they were just
be added in direct proportions with gold content in a bath. So if you know the
gold content, you have the idea how much brightener you will add.]

Hope this helps

Jonathan
Fairchild semiconductor
Package Technology Group








Jack Petyak <[log in to unmask]> on 03/29/2000 08:57:03 AM

Please respond to "\"TechNet E-Mail Forum.\" <[log in to unmask]>,        Jack
      Petyak" <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Jonathan A Noquil/Cebu/Fairchild)
Subject:  [TN] Plating processes




Anyone have any input about how to analyze carriers
and brighteners in plating baths? What about potential
problems with gold plating?

I'll probably have more plating process questions as I
get deeper into my project so if the experts can offer
any advice I'd appreciate any help.

Thanks, Jack

__________________________________________________
Do You Yahoo!?
Talk to your friends online with Yahoo! Messenger.
http://im.yahoo.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2