TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Klasek <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 17 Mar 2000 09:37:38 +1100
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
Whatever you do , if any QA mgr will suggest you PENCIL ERASERS ; desist ,
go to archives ; we've had a discussion on this bad habit with Dave Hillman
not so long ago .

This is the case of cure worst than illness , address the process .

paul

-----Original Message-----
From: David Kim [mailto:[log in to unmask]]
Sent: Friday, 17 March 2000 6:16
To: [log in to unmask]
Subject: [TN] stain&gold plating



 I am looking for suggestions on "How to remove a stain on gold surface and
why does a stain happen on gold surface after plating?"

 In electroless Ni/immersion Au plating, I have found many stain problems
after plating. Threre are varied shapes of stains such as a spot, a line,
and an irregulare shpae.

 Anyone who can suggest a better idea?

 thank you!

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2