correct, if 20% or more of the trace is missing, for whatever reason, i
would consider it a reject. definitely communicate back to your vendor on
this issue (i'm sure you will), especially is its repeating itself panel
after panel. sounds like contamination or a flaw in the artwork..
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, March 14, 2000 10:52 AM
To: [log in to unmask]
Subject: [TN] Etched "Notches" or "Nicks" in copper traces
Hi ya'll!
I gotta board here that has a problem with the traces, it looks something
like this:
Nick in the Trace
|
V ___
________________ ___,/ \
\_/ | <-------This is supposed to
be a via..
______________________, |
\___/
(I hope my "ascii cad" conveys what I'm trying to show) Reading the
IPC-A-600F at 2.10.1.1 Conductor width it says for class 2 and 3 it is
acceptable when;
"Any combination of isolated edge roughness, nicks, pin holes, and scratches
exposing the base material that reduces the conductor width by 20% of the
minimum value or less."
So I'm reading this correctly, if the nick reduces the trace width by more
than 20% of the overall trace width, it is a reject...right? This "nick"
seems to have been etched like this...it's at the same place on the same
board that's in a 4-up panel. The other 3-boards in the panel don't have
this
"nick". Booger on the artwork or something huh?
Just want to be sure...
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|