Brian: You left out the one which is always overlooked > Dupont!!
If Jonathon needs HMP alloys in the 250 -300C region it might be worth contacting them.
Surprisingly, their thick film people have some quite handy hmp solder pastes which are lead
free,
they think of them as high strength solders or low temp brazes and are buried in the back of
their thick film ink literature.
One caution: Dupont is not a cheap company and the alloy constituents are relatively exotic.
Mike
----- Original Message -----
From: Brian Ellis <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 02, 2000 8:40 AM
Subject: Re: [TN] High Temp solders
> Also Alpha Metals, Heraeus, Multicore Solders, Promosol etc., you name it, they have
> it.
>
> Brian
>
> Jonathan A Noquil wrote:
>
> > Hello Guys
> >
> > anybody knows about suppliers for high temp solder paste?
> > And that is lead free?
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> > information.
> > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700 ext.5315
> > ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|