Phil, it sounds like the "new guy" needs to see the results of your
investigation. What good is the staking if it is cracked and/or not properly
adhering to the parts. Obviously the "new guy" needs to take some lessons
from the "old timer" who has been through it! What does upper management
say? What does the customer say? Are they willing to take the risk of
failure to save a few pennies of processing time. Can you company afford to
risk its reputation and good name by shipping an inferior product? I would
think not. Show the new guy why and how you arrived at your position.
Remember "hindsight is always 20/20".
Ron Dieselberg
BAE SYSTEMS Cincinnati Electronics Corp.
-----Original Message-----
From: phil bavaro [mailto:[log in to unmask]]
Sent: Monday, March 20, 2000 17:05
To: [log in to unmask]
Subject: [TN] Electrolytic Capacitor Staking Requirements
OK, I know, I know. Why is anyone still using thru hole parts which have to
be bonded to the board......!!
Well. all I can say is that we are and the question I have for this group
is what are the requirements for how much and how high.
Here's the background info:
An automotive electronics circuit card has about seven very tall
electrolytic caps on it which need to be secured to the board so that the
vibration does not sever the two leads on these parts. Historically I have
always asked that these be bonded 360 degrees around the perimeter and a
minimum of 50%, up to a maximum of 100% of the height of the part using a
thixotropic UV cure adhesive. This way the part could not bend or move at
all.
Using this criteria, I have never seen a failure as a result of the bonding.
Here's the problem:
A new engineer decides to minimize the adhesive amount (due to cycle time
of course) so that just it connects the board and the bottom of the part
only (maybe as high as .15" total which only allows about .10" of contact
to the body of the part. These parts are .75" tall. The new engineer
feels justified because the products which were bonded this way made it
thru a HALT test exposure without electrical failures.
I look at the assemblies which are supposedly OK and find that the adhesive
has broken loose from the pwb on at least five out of the seven parts and
what is remaining on the parts have fracture lines as well.
I consider this condition unacceptable and feel that after environmental
testing, adhesive bonding should remain intact 100%.
Am I right or should I yield since the assemblies made it thru the HALT
testing? What bonding requirements do you impose for these type of parts
All comments are welcome.
-----------------------------------------------------
Click here for Free Video!!
http://www.gohip.com/freevideo/
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|