Subject:
From:
Franklin Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 16 Mar 2000 17:04:55 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (81 lines)
Hey now, I only suggested the eraser as an indicator for the type of stain,
i.e. surface, plating contaminate, etc.

I wrote: "...take an ordinary pencil eraser and try to remove the stain, if
it comes off you'll probably have good results with a solution clean."

Notice I followed up with a solution clean.

This lowly Quality Assurance Manager knows a couple things now...

~grinning~

Franklin D Asbell

----- Original Message -----
From: Paul Klasek <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 16, 2000 2:37 PM
Subject: Re: [TN] stain&gold plating


> Whatever you do , if any QA mgr will suggest you PENCIL ERASERS ; desist ,
> go to archives ; we've had a discussion on this bad habit with Dave
Hillman
> not so long ago .
>
> This is the case of cure worst than illness , address the process .
>
> paul
>
> -----Original Message-----
> From: David Kim [mailto:[log in to unmask]]
> Sent: Friday, 17 March 2000 6:16
> To: [log in to unmask]
> Subject: [TN] stain&gold plating
>
>
>
>  I am looking for suggestions on "How to remove a stain on gold surface
and
> why does a stain happen on gold surface after plating?"
>
>  In electroless Ni/immersion Au plating, I have found many stain problems
> after plating. Threre are varied shapes of stains such as a spot, a line,
> and an irregulare shpae.
>
>  Anyone who can suggest a better idea?
>
>  thank you!
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2