TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Date:
Fri, 3 Mar 2000 14:22:52 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (141 lines)
"Ingemar Hernefjord (EMW)" wrote:

> Aegreto Brianus, dum anima est, spes esse dicitur!
> Not pig latin. Means approx "Said for Brian, a crazy person, but there is hope as long as there is life."

Actually, I always thought 'dum anima est' meant 'he is a dumb animal'. Errare humanum est.

>
> Acta est fabula, ergo plaudite et dulce perdidi.

Thanks.

My Latin is becoming somewhat strained, considering that the last time I opened a Latin book was in 1945! 55 years is amply
long enough to have forgotten twice as much as I ever learned.

>
> .-- . / -- .- -.-- / .... .- ...- . / - --- / ..- ... . / .-.. .- - .. -. / .. -. / --- - .... . .-. / --.- .-. . --.- /

The last time I touched a Morse key must have been about 1953, in the Army, so that is a little rusty as well. However, I did
fine up until the last word, QREQ????? Believe it or not, I have a Merchant Marine Radio Operators ticket (1950) so I must
have been able to do 25 wpm then: now 0,25 wpm :-) In my mispent youth, I was also a radio ham (some say I still am a ham),
GM3GUC and ZC4BN. Happily, the Morse code is now officially obsolete (as from last year).

>
> Over and out / Ingemar
> Just had to do this, it's Fryday and soon time for both this and that. Yeaahooo!

Efharisto polee, Ingemar, kai yia sou

Brian

>
>
> Oh well! You asked for it, Ingemar, to misquote Virgil:
> Ecce, igitur, hic canis non gelidus, Brianus, de montibus humor laborat.
>
> Liberally translated for the non-Latin scholars this will give:
> Lo and behold, therefore, this co-o-o-ol dog, Brian, tumbles down the mountains by way of a joke.
> :-)
>
> Brian
>
> "Ingemar Hernefjord (EMW)" wrote:
>
> > Couldn't resist teasing Brian. "vixi" means "stumbled". I guess Brian will give back with 200%. (more giggle) / Ingemar
> >
> > Subject: Re: [TN] How to detect contamination on metal surface
> >
> > Help me out Ingemar,
> > My poor American education did not include Latin-what is "vixi"? I'm sure
> > it's a very clever little joke.
> >
> > Timothy Reeves
> > ECD Circuit Board Division
> > 13626 South Freeman Road
> > Mulino, OR 97042
> > [log in to unmask]
> > (503) 829-9108 (800) 228-8198  FAX (503) 829-5482
> >
> > > ----------
> > > From:         Ingemar Hernefjord (EMW)
> > > Sent:         Thursday, March 2, 2000 6:12
> > > Subject:      Re: How to detect contamination on metal surface
> > >
> > > Veni vidi vixi (giggle, giggle)
> > > Ingemar
> > >
> > >
> > > Hi, all!
> > >
> > > OK, I may have been too categorical in my previous post. It may work for
> > > some depending
> > > on the degree of cleanliness they require, the purity of the water, the
> > > substrate
> > > material and the surface finish of the material under practical
> > > conditions. I maintain
> > > though that the basic premisses of the test are flawed and that universal
> > > application
> > > of it may lead to problems and disappointments - or worse.
> > >
> > > Caveat utilisator
> > >
> > > Brian
> > >
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> > the body:
> > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > To unsubscribe:   SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> > information.
> > If you need assistance - contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700 ext.5315
> > ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2