Couldn't resist teasing Brian. "vixi" means "stumbled". I guess Brian will give back with 200%. (more giggle) / Ingemar
Subject: Re: [TN] How to detect contamination on metal surface
Help me out Ingemar,
My poor American education did not include Latin-what is "vixi"? I'm sure
it's a very clever little joke.
Timothy Reeves
ECD Circuit Board Division
13626 South Freeman Road
Mulino, OR 97042
[log in to unmask]
(503) 829-9108 (800) 228-8198 FAX (503) 829-5482
> ----------
> From: Ingemar Hernefjord (EMW)
> Sent: Thursday, March 2, 2000 6:12
> Subject: Re: How to detect contamination on metal surface
>
> Veni vidi vixi (giggle, giggle)
> Ingemar
>
>
> Hi, all!
>
> OK, I may have been too categorical in my previous post. It may work for
> some depending
> on the degree of cleanliness they require, the purity of the water, the
> substrate
> material and the surface finish of the material under practical
> conditions. I maintain
> though that the basic premisses of the test are flawed and that universal
> application
> of it may lead to problems and disappointments - or worse.
>
> Caveat utilisator
>
> Brian
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|