TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Marsico, James" <[log in to unmask]>
Date:
Fri, 31 Mar 2000 07:22:13 -0500
MIME-Version:
1.0
X-To:
"Misner, Bruce" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Marsico, James" <[log in to unmask]>
Parts/Attachments:
text/plain (164 lines)
The LCCs we use are all pre-tinned.  If not received that way, we send them
out to a tinning house.
Thanks,
Jim M.


        -----Original Message-----
        From:   Misner, Bruce [SMTP:[log in to unmask]]
        Sent:   Thursday, March 30, 2000 11:52 AM
        To:     [log in to unmask]
        Subject:        Re: [TN] SMT DEFECT RATES (DPMO)

        Jim,

        I would have to agree with Ed. Pre-tinning should help immensly,
just be
        careful of leaching, although it shouldn't be a concern unless you
plan on
        recycling LCC's off reject boards.

        Bruce Misner

        > ----------
        > From:         Edward J. Valentine[SMTP:[log in to unmask]]
        > Reply To:     TechNet E-Mail Forum.;Edward J. Valentine
        > Sent:         Thursday, March 30, 2000 11:09 AM
        > To:   [log in to unmask]
        > Subject:      Re: [TN] SMT DEFECT RATES (DPMO)
        >
        > Jim - A side question - Are you pretinning your LCC's?  If not,
you should
        > seriously consider the pre-tinning operation, especially if the
Gold
        > castellations are contaminated. You would know this ahead of time
by
        > verifying the coverage after pre-tinning. And, in my experience,
the
        > pretinning produced significantly better soldering results even
though you
        > are adding additional process steps. Ed/
        >
        > Ed Valentine
        > Electronics Manufacturing Solutions
        > 8612 Mourning Dove Road, Raleigh, NC 27615
        > Phone: (919) 270-5145, Fax: (919) 847-9971
        > Email: [log in to unmask]
        > Website: http://www.ems-consulting.com
        >
        > ----- Original Message -----
        > From: Marsico, James <[log in to unmask]>
        > To: <[log in to unmask]>
        > Sent: Thursday, March 30, 2000 10:29 AM
        > Subject: [TN] SMT DEFECT RATES (DPMO)
        >
        >
        > > Dear Technet:
        > >
        > > I've been tasked by my superiors to query industry to find out
what
        > other
        > > electronic assemblers are yielding off of their surface mount
line.  To
        > > compare apples to apples, here are my specifics:
        > >
        > > We assemble SMT for military/high rel.  The majority of the
parts are
        > > ceramic leadless chip carriers  (LCCs) and ceramic chip
components
        > > (resistors, caps, diodes).  We're starting to track solder
defects more
        > > closely when the assemblies come right off the line, and we
don't like
        > what
        > > we see.  The major anomaly is insufficient solder fillet on the
LCCs.
        > > (There could be one joint insufficient out of 20. By the way,
solder
        > paste
        > > deposits are perfect!)  Whether or not these are actually
defects is
        > under
        > > discussion.
        > >
        > > What I'd like to know is:
        > > 1)      What kind of defect rates (PPM) are others, building
similar
        > > assemblies, getting from their SMT lines.
        > > 2)      Does anyone experience insufficient solder on LCCs?
        > >
        > > Thanks,
        > > Jim M.
        > > AIL Systems Inc.
        > > 631-595-5879
        > >
        > > ##############################################################
        > > TechNet Mail List provided as a free service by IPC using
LISTSERV 1.8c
        > > ##############################################################
        > > To subscribe/unsubscribe, send a message to [log in to unmask]
with
        > following text in
        > > the body:
        > > To subscribe:   SUBSCRIBE TECHNET <your full name>
        > > To unsubscribe:   SIGNOFF TECHNET
        > > ##############################################################
        > > Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for
        > additional
        > > information.
        > > If you need assistance - contact Keach Sasamori at
[log in to unmask] or
        > > 847-509-9700 ext.5315
        > > ##############################################################
        >
        > ##############################################################
        > TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        > ##############################################################
        > To subscribe/unsubscribe, send a message to [log in to unmask] with
        > following text in
        > the body:
        > To subscribe:   SUBSCRIBE TECHNET <your full name>
        > To unsubscribe:   SIGNOFF TECHNET
        > ##############################################################
        > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
        > additional
        > information.
        > If you need assistance - contact Keach Sasamori at [log in to unmask]
or
        > 847-509-9700 ext.5315
        > ##############################################################
        >

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Keach Sasamori at [log in to unmask] or
        847-509-9700 ext.5315
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2