TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brian Ellis <[log in to unmask]>
Date:
Mon, 27 Mar 2000 11:52:17 +0100
Reply-To:
Alan Brewin <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Alan Brewin <[log in to unmask]>
Parts/Attachments:
text/plain (139 lines)
Dear Brian/Grant,

Amen. Supporting customers using conformal coating products, as I do, this
is one of the most commonly asked questions, and I agree with Brian's
answer.

In fact this is why we use SIR as a research tool in development and many
people who chose to coat over no-clean validate their mix of process
chemicals and process settings with SIR.

Other residues can also come from handling, especially if staff have been
used to a process where the boards were cleaned in the past.

Regards,

Alan Brewin.
Concoat Ltd.

-----Original Message-----
From: Brian Ellis <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 25 March 2000 13:56
Subject: Re: [TN] Coating of assemblies with no clean fluxes


>Grant
>
>As a general rule, coating over flux residues is dangerous IMHO. There
>may be a few exceptions, but these are generally unavailable to the
>common mortal. Let us look at what is left on a board:
>- unmodified flux residues (it is BS to say that they are "burnt off"),
>possibly a dibasic carboxylic acid, maybe with organic halides, maybe
>with rosin or something similar
>- ionic salts (tin, lead, copper etc. carboxylates, halides, etc.)
>- polymerised flux residues
>- contaminants from boards and components, which may include
>inadequately washed water-soluble fluxes etc.
>- residues from rheological modifiers, maybe glycols etc. (hygroscopic)
>
>If you leave all these on the board and then coat over them, you are in
>DEEP trouble.
>
>One possible exception is where the flux is a fairly concentrated adipic
>acid type and where the coating is an epoxy which requires adipic acid
>for cross-linking, but this is hairy a) because it will be impossible to
>guarantee stoichiometry, b) it will not be homogeneous and c) you still
>have all the other gunge under the coating. The automobile industry use
>this technique (ever wonder why there are so many modern cars with
>failures of the electronics?).
>
>The short answer is your vendor is a liar.
>
>Brian
>
>
>Grant Emandien wrote:
>>
>> Hi all,
>>
>> The debate on cleaning of fluxes as well as the use no-clean fluxes seems
to
>> hang around forever. We have been informed by our solder an flux supplier
>> that assemblies with no clean fluxes can be conformally coated without
the
>> need to clean the boards.
>>
>> The argument is that the high temperatures of the reflow oven 'burns off'
>> the active ingredients, leaving only inactive residues. These flux
residues
>> do not have to be cleaned and can supposedly be coated. The rep. believes
we
>> are taking a backward step by possibly opting to use water-based flux. Is
>> this pure sales talk?
>>
>> Is anyone able to offer any advice or insight, or been able to assess the
>> environmental and electrical performance of such assemblies.
>>
>> Regards
>> Grant
>>
>> ##############################################################
>> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>> ##############################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>> the body:
>> To subscribe:   SUBSCRIBE TECHNET <your full name>
>> To unsubscribe:   SIGNOFF TECHNET
>> ##############################################################
>> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>> information.
>> If you need assistance - contact Keach Sasamori at [log in to unmask] or
>> 847-509-9700 ext.5315
>> ##############################################################
>
>--
>Brian Ellis
>Protonique SA
>PO Box 78
>CH-1032 Romanel-sur-Lausanne, Switzerland
>Voice: +41 21-648 23 34 Fax: +41 21-648 24 11
>E-mail: [log in to unmask]
>URL: Technical and consultancy divisions:
>       http://www.protonique.com
>     Web services division:
>       http://www.protonique.com/webserv
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2