Understand, especially with through hole mounting and the problems with
blow holes. But I believe Dewey was talking about SMT. With thin
coatings in a humid environment I'm sure the copper can become oxidized
and create soldering problems. What about moisture after assembly and
prior to say conformal coating?
Rick
>-----Original Message-----
>From: Alain Savard [SMTP:[log in to unmask]]
>Sent: Wednesday, March 22, 2000 7:16 AM
>To: [log in to unmask]
>Subject: Re: [TN] Baking FR4 boards
>
>There is no actual requirement, it is more of a factual moisture absorption
>effect. Polyimide absorbs water a lot faster then FR4. I don't know of much
>of a problem with using FR4 up to 6 months old. After that we may recommend
>prebake. This is an in-house specification, I don't know of any IPC
>specification for it.
>
>
>
>Alain Savard, B.Sc.
>Chemical Process Analyst
>CAE Electronics Ltd.
>e-mail: [log in to unmask]
>
>-----Original Message-----
>From: Dewey Whittaker
>Subject: Re: [TN] Baking FR4 boards
>
>
>"Howieson, Rick" wrote:
>Out of curiosity, where are these requirements stated?
>Rick
>>-----Original Message-----
>>From: Dewey Whittaker
>>Subject: Re: [TN] Baking FR4 boards
>>
>>Alain Savard wrote:
>>
>>> Isn't the 72 hours before bake a requirement for polyimide instead of
>FR4?
>>>
>>> Alain Savard, B.Sc.
>>> Chemical Process Analyst
>>> CAE Electronics Ltd.
>>> e-mail: [log in to unmask]
>>>
>>> -----Original Message-----
>>> From: Dewey Whittaker
>>> 1. Typically, for multi-layer (6-8 layers), FR4, SMT boards stored in an
>>>air
>>>
>>> conditioned environment at about 50+/- 10% RH, how many months would you
>>> allow
>>> to pass before you would recommend baking them prior to reflow?
>>> 2. What would be your bake cycle?
>>> Thanks,
>>> Charlie B.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|