TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Jeff Hempton <[log in to unmask]>
Date:
Fri, 17 Mar 2000 08:54:52 -0500
Content-Type:
multipart/mixed; boundary="IMA.Boundary.7451033590"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jeff Hempton <[log in to unmask]>
Parts/Attachments:
text/plain (982 bytes) , text/plain (989 bytes)
     Franklin,
     Thanks to everyone for your responses on this so far.
       Do I understand correctly that you use a standard LPI and totally
     cover, or "tent" over the vias, then UV cure, then repeat on other
     side? And the UV cure keeps the LPI from creating a blow-hole during
     assembly? Or are you UV curing a separate "plug" material, then LPI
     covering?
     Jeff Hempton
     UT Electronic Controls


______________________________ Forward Header __________________________________
Subject: [TN] To plug or not to plug
Author:  Franklin Asbell <[log in to unmask]> at Internet
Date:    03/17/2000 7:22 AM


One solution we found to the LPI plugging issue is:

STEP 1: Coat, tack, image, cure, then follow up with a UV cure one one side.
STEP 2: Repeat step 1 for the opposite side

Yes, this is somewhat time consuming; however, it has worked out great in the
few exceptional jobs we needed to do this on.

I welcome all other reasonable solutions.

Thanks,

Franklin D Asbell



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2614.3500" name=GENERATOR> <STYLE></STYLE> </HEAD> <BODY bgColor=#ffffff> <DIV><FONT face=Arial size=2>One solution we found to the LPI plugging issue is:</FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT face=Arial size=2>STEP 1: Coat, tack, image, cure,&nbsp;then follow up with a UV cure one one side.</FONT></DIV> <DIV><FONT face=Arial size=2>STEP 2: Repeat step 1 for the opposite side</FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT face=Arial size=2>Yes, this is somewhat time consuming; however, it has worked out great in the few exceptional jobs we needed to do this on.</FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT face=Arial size=2>I welcome all other reasonable solutions.</FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT face=Arial size=2>Thanks,</FONT></DIV> <DIV>&nbsp;</DIV> <DIV><FONT face=Arial size=2>Franklin D Asbell</FONT></DIV></BODY></HTML>