Rick Howieson & Others:
Rick, you ask how thick our gold was . . . I misled everyone in the type of
plating . . . it's not immersion but rather electroplating. Our spec is
6-10 and we are getting or got, 20-30 on some boards. These are the boards
we would like to remove some gold if possible.
I understand that electroplating your thickness depends on time rather than
ion for ion in immersion plating.
Thanks
Ron
##############################################################