For FR4 boards we use a Westek inline water cleaner with Kyzen Aquanox in
it. Getting flux out of ceramic boards is tough especially if it is baked or
heated in. I saw a demonstration once at EMC in Doylestown,PA in which we
tried to clead bake on RMA flux out of a ceramic PWA. We tried hot
saponifier, and aquanox spray but the absorbed flux did not completely come
out. What did the trick was hot alcohol spray. The board came out of the
chamber pure white.
-----Original Message-----
From: Cecilia Alkhagen (EMW) [mailto:[log in to unmask]]
Sent: Wednesday, March 01, 2000 11:21 AM
To: [log in to unmask]
Subject: [TN] Solvent Cleaning
Hello!
Could anyone tell me the most effective way of cleaning RMA-flux on
FR4-boards as well as ceramic substrates. Both inline and batch cleaning is
of interest.
Component stand-off is 0.04mm in some cases and micro-BGA:s are soon in the
production line.
Cecilia Alkhagen
Ericsson Microwave Systems AB
SE-431 84 Mölndal
Sweden
Phone: +46 31 747 02 88
Fax: +46 31 747 26 35
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|