hi,
not all alumina packages are white. we use many alumina packages that are brownish. you may say that there is something other than aluminal in these packages that make them brownish, but the fact is that in this industry, when you say a package is alumina, it doesn't mean it's white.
phil
-----Original Message-----
From: Carey Pico [mailto:[log in to unmask]]
Sent: Monday, February 28, 2000 9:30 PM
To: [log in to unmask]
Subject: Re: [TN] Color of ceramic BGA's
Of course. Alumina is white
Carey
-----Original Message-----
From: d. terstegge <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Monday, February 28, 2000 8:54 AM
Subject: [TN] Color of ceramic BGA's
Hi Technetters,
During acceptance testing of our new pick&place machine we ran into a
problem: the vision system can't see the solderballs on the white ceramic
substrate of our Topline dummy-CBGA's. It's just not supported.
I have never used CBGA's in our production, and I was wondering if real-life
CBGA's can have this same color.
Kind regards
Daan Terstegge
Unclassified mail
Personal website: http://surf.to/smtinfo
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|