Michael,

Which IPC spec are you referring to?

Martin
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
21/02/00 08:26
>TechNetters:
>
>IPC specs recommend re-baking if PCBs are stored at over 40% humidity for more
>than 5 days.
>
>What, roughly, is the shelf life before re-baking is needed for lower
>humidities, e.g. NW Europe?
>
>Tks. in advance,
>
>Michael
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2