TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Bob Crain <[log in to unmask]>
Date:
Fri, 4 Feb 2000 00:59:26 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Thomi <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Parts/Attachments:
text/plain (60 lines)
Hi Bob,

how about clinching the leads for a defined standoff? This would also give
you a well defined strain relief. Suggestions about the mounting and
clinching geometry are displayed in IPC-A-610.

Schön' Gruss, best regards,

Thomas Ahrens, Memellandstr. 8, D-24598 Boostedt
Tel. ++(49) (0) 4393 97769   e-mail [log in to unmask]
Bitte beachten - please note:
- Mails groesser als 2 MB werden nicht angenommen
- messages larger than 2 MB will not be downloaded
-----Ursprüngliche Nachricht-----
Von: Bob Crain <[log in to unmask]>
An: [log in to unmask] <[log in to unmask]>
Datum: Donnerstag, 3. Februar 2000 23:39
Betreff: [TN] Temporary stand offs for wave solder


We are converting some old hand solder aerospace PCA designs to wave solder.
The transistors and CKR05 type capacitors need temporary stand offs.

We cannot use standard dissolvable spacers because we use alcohol solvent
cleaning and are not allowed to use water.

Suggestions? One thing I would like to consider is a high temperature,
non-silicone, non-sulfur rubber sheet in thicknesses of .030" and .050." Any
ideas for the best material to use? Are there any removable clips that fit
over the parts to hold them up?

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2