Glenn: Add a UV tracer to your flux.If flux residues are present after
cleaning they will fluoresce when exposed to a UV(blacklight)source.
I have used Rhodamine B in the past with water soluble fluxes.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-356-6076
-----Original Message-----
From: Glenn Pelkey [mailto:[log in to unmask]]
Sent: Tuesday, February 22, 2000 10:31 AM
To: [log in to unmask]
Subject: [TN] Residual Flux Indicator
Hi all,
Anyone familiar with a dye that can help indicate the presence of
residual flux? I was just talking with another engineer who mentioned a
material called "Bromthymol Blue" that he used to use. Is it still
available
or is there's something better?
The reason I ask is we have these small "Bumped Chip" devices on a
board. Historically there has been a problem with residual flux under these
components, not visible to inspection and averaged out with ROSE test. We
want to destructively remove a few and see how effective the cleaning
process
is.
Thanks for your help,
Glenn
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|