Hi
Here is some precisions that could maybe help you to help me !!
* Gold plating thickness : Minimum 0.000030 in
* Gold hardness: 130-200 Knoop
* Under plate type and thickness : Minimum 0.000100 in of Ni on 0.001 in
of Cu
* Office environment and no lubricant
Is it also possible for you to tell me where does your data come from
(25-100 insertions) ?
Does it come from the connectors datasheets ? If so, is it related to
`spring` resistance only or gold abrasion on PCB or both ??
Thank in advance for your collaboration
Alain
______________________________
At 10:51 PM 2/4/2000 -0800, you wrote:
> Alain,
>The number of insertion life for a gold contact systems depends upon the
>following factors- Gold plating thickness Type of gold soft vs hard
>Under plate type and thickness Contact spring material ( BeCu,
>Phophorbronze etc.) Contact force (affects insertion force and wear)
>Contact geometry Use of contact lubrication Contact cleanliness (
>debris and particulate matter) Plating porosity Use environment (
>temperature, humidity, gases, vibration etc.) < 25 -100 insertions before
>contact resistance degradation. Alain Giguere wrote: Do you know what is
>the maximum number of insertions a gold contact (on a
>PCB) can hold until it is no longer reliable (or wears out)?
>_______________________________________________ Alain Giguere
>Quality Department
>Matrox Electronic Systems LTD. Tel: (514) 969-6000 ext.2978
>e-mail: [log in to unmask]
--
>____________________________________
>Regards,
>Pratap Singh Tel./Fax: 512-255-6820,
>e-mail: [log in to unmask] or [log in to unmask]
>
Do you know what is the maximum number of insertions a gold contact (on a
PCB) can hold until it is no longer
reliable (or wears out)?
Alain
_______________________________________________
Alain Giguere
Quality Department
Matrox Electronic Systems LTD.
Tel: (514) 969-6000 ext.2978
e-mail: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|