The square pads will give you better release of the paste, also the square
pads will help you see if the bga has reflowed properly when you x-ray them.

-----Original Message-----
From: Larry Jindra [mailto:[log in to unmask]]
Sent: February 2, 2000 10:34 AM
To: [log in to unmask]
Subject: [TN] MiniBGA pad conflicts


I'm a little confused.  J-STD-013 recommends 22 mil pads for 1.00mm pitch
BGAs, but the guideline for IPC7527 suggests 15 mil round pads with a square
paste opening.  Is anyone out there having good luck with one or the other?
Why the large disparity?

Thanks-

> Larry Jindra
> TRW/Avionics Systems Division
> mailto:[log in to unmask]   ph (858) 592-3424   fax (858) 592-3606
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2