Good afternoon Technet,
We are looking for a referral for a customer that requires the
following:
Gold plate on top side only (selective)
Gold plate over Nickel Plate 6-12 microns (must be a typo)
Gold plate thickness 2-4 microns (appears to be immersion)
Gold plate hardness 130-200 (knoop scale)
This is a little 4 layer, 1 oz copper all thru. It looks like a touch
keypad.
Anyone know where to get this one made?
Thanks in advance for any input, we'll forward on all names to the end
user.
Anne Ledger
EMDS, Inc.
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|