In a message dated 02/10/2000 12:41:18 PM Central Standard Time,
[log in to unmask] writes:
<< Hi all,
I'm trying to determine the "outer limits" of stencil thickness vs.
aperature diameter at very small diametr (.006" - .010") Can anyone share
some experience?
Thanks in advance,
Ed Popielarski
QTA Machine
10 Mc Laren, Ste. D
Irvine, Ca. 92618
Ph: 949-581-6601
Fx: 949-581-2448
http://www.qta.net
Check out our BGA Baller and Process Equipment Services! >>
Hey Ed!
.006 -.010" diameters!? Hoo-doggies, that's getting teeny-tiny! Flip chip? I
haven't had any other experience except for when I worked for Zevatech. We
built a little keychain board that had a flip chip on it and if I remember
correctly, they had 6-mil pads. The stencil was like aluminum foil, only 2 or
3 mils thick...you could crease it with your thumb-nail. The normal 1.5
aperture width to thinkness ratio really doesn't apply to circular openings
though...to much sidewall friction to overcome for the paste to release from
the stencil good. That's why I always do square apertures on microbga, the
paste releases better from the stencil.
I just built a prototype board last week that had a 256-ball microbga...I
used a 4-mil stencil...and the pads on the board were giant compared to what
you're talking about...they were 20-mil. I used square openings and it worked
out fine...
So in my estimation, .006 -.010" diameter openings I don't think you'll get
much thicker than 3-mils and get good paste release.
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|