Hi Phillip,
We've been making stuff with double treat for a while and haven't run into
any delam trouble. You do need to watch the handling procedures -
protecting the panels from bare hands. Although when it does (rarely) occur
the smudges are quite apparent. On the plus side you get to skip the oxide
process.
Hans
~~~~~~~~
Hans M. Hinners
Materials (& Process!) Engineer
Warner Robins - Air Logistics Center/Avionics Production Division
Manufacturing Branch (LYPME)
380 Second Street, Suite 104 (Building 640)
Robins AFB, GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7164 (Fax)
mailto:[log in to unmask]
> -----Original Message-----
> From: Spann, Phillip J (S3) [SMTP:[log in to unmask]]
> Sent: Tuesday, February 22, 2000 10:36
> To: [log in to unmask]
> Subject: [TN] Double treat copper
>
> We are a small PCB shop producing multilayer boards. Does anyone know
> any advantages or
> disadvantages in using double treated copper as opposed to standard
> "slick"
> copper for inner layers.
> We are concerned about boards delaminating after some time in the field.
> Currently we use standard
> FR4 with a slick finish and do not have any known problems with
> delamination, but are not 100% sure
> about the product over time. Thanks in advance for any input.
>
>
> Phillip Spann
>
> S3, Inc.
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|