Hi Jason and All -
You don't mention what class wire insulation is involved in this
application, or what its end service environment is, so I think that leaves
all of us at a bit of a disadvantage.
Flying blind, I would suggest that you consider a brush touch-up with a
conformal coating, suitable to your end use and compatitible with the basic
insulating material. You may need to do a bit of manual cleaning and
removal of flux, etc., prior to the application. Air curing the touch-up
material for a while (generally an hour or less) will normally allow
solvents to exhaust and let the material settle into the windings. A low
grade vacuum may also help in this application. You may also want to warm
the winding slightly, prior to coating application to help flow, and exhaust
the cleaning fluids.
The whole issue goes back to providing an electrical insulating compound
with suitable dielectric properties for the design.
Regards - Kelly
-----Original Message-----
From: Jason Gregory <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Sunday, February 27, 2000 9:20 AM
Subject: [TN] transformer coating issues
>Hello technet,
>
>Hopefully there are some bored Sunday e-mail surfers out there.
>We have an issue with acceptability standards on coiled transformers and
the issue is this: all of our red-coated x-formers have areas where the
protective coating is nicked or the heat from the iron during rework is
peeling the coating back and exposing copper. Is there an IPC standard
dictating acceptability? Please help!!
>
>Jason Gregory
>Production Manager
>Electrospec
>8626 Westpark
>Houston, TX. 77063
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|