TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 24 Feb 2000 08:28:48 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Douglas Pauls <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
In a message dated 02/23/2000 4:28:52 PM US Eastern Standard Time,
[log in to unmask] writes:

> but your local jeweler/supply does sell silver and gold cleaning compounds
>  and aids .
>

Yes, they do.  But be very cautious.  Most are too aggressive or have
surfactant compounds that are detrimental if  not completely removed.  I had
a client once who asked if they could use Tarn-X as a flux.  I shudder even
thinking about it.

Doug Pauls

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2