My team has been very successful using this process to avoid solder skips on
boards with wave solder design rule violations. Incidentally, I run a
temperature profile with a marginal time above liquidus to maintain
throughput in a very short four zone oven. The fresh, albeit grainy, solder
joints wet nicely in the wave and the final results are excellent.
Regards,
Brad
-----Original Message-----
From: Murugan Vasudevan [mailto:[log in to unmask]]
Sent: Tuesday, February 15, 2000 7:24 AM
To: [log in to unmask]
Subject: [TN] Cure and Reflow
Hi Technetters,
Just wondering if anyone of you have done simultaneous
cure of SMD adhesives and reflow of solder paste in
the same pass. Any information/leads on any previous
experiences with this process will be very helpful.
Thanks,
Murugan.
__________________________________________________
Do You Yahoo!?
Talk to your friends online with Yahoo! Messenger.
http://im.yahoo.com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|