Rick,
Be careful. Measling can be a source of reliability problem when it bridges two
conductors. Measling becomes 'A' type defect ( Critical function -causing rejection)
when two conductors of different polarity are bridges. If glass fibers become visible
in a measled spot, that is also a cause for concern.
Send pictures of measled board for further discussion if you like.
"Howieson, Rick" wrote:
> IPC states measling is not cause for rejection. Anyone out there know
> where I can get supporting data that documents testing performed to come
> to this conclusion? All help is appreciated.
>
> Rick Howieson
> http://www.gt-corp.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
--
____________________________________
Regards,
Pratap Singh
Tel./Fax: 512-255-6820,
e-mail: [log in to unmask] or [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|